Glossary · Wafers and substrates

Dimple

A dimple is a shallow, dish-shaped depression on a surface, the same word used for the hollows on a golf ball. In semiconductors it refers to a local depression defect on the wafer or chip surface, and also to processes that grind such a depression on purpose, most notably in preparing samples for transmission electron microscopy (TEM).

Also called: dimple defect, dimple grinding

Diagram


Meanings of dimple: a wafer surface depression defect and TEM sample preparation

Click anywhere to zoom in there. Scroll to zoom, drag to move

In everyday English, a dimple is a small hollow.

Dimples as a wafer defect


As a wafer defect, a dimple is a very shallow depression a few millimetres across that appears on the surface after polishing. Causes include uneven pressure during polishing, local conditions of the wafer holder or polishing pad, and defects inside the crystal.

A dimple can be too shallow to see by eye and still matter. Advanced lithography has a very small depth of focus, so even a slight local depression can put part of the exposure out of focus. Dimples are therefore controlled as part of nanotopography, the height variation of the wafer surface over a range of a few millimetres, measured with optical flatness and surface inspection tools.

In device processing, the depression that forms when chemical mechanical polishing (CMP) removes metal lines or pads faster than the surrounding dielectric is called dishing, and is usually treated separately from dimples.

Dimpling on purpose


In TEM sample preparation, dimple grinding polishes a dish into the centre of the sample so that only the middle is thin. The sample is then finished by ion milling until it is thin enough for the electron beam to pass through. The word is also used in packaging and thermal design, where small hollows are formed to control how solder spreads or how air escapes.

Japanese companies involved


  • Japanese silicon wafer makers such as SUMCO specify and inspect surface flatness, including nanotopography, on polished wafers for advanced lithography.
  • SUMCO · Silicon wafers
  • Lasertec · EUV mask and mask blank inspection

FAQ


How is a dimple different from dishing?

A dimple is a general local depression on a surface, most often a defect on a polished bare wafer. Dishing is the dish-shaped recess of metal lines or pads after CMP, and it depends on the pattern layout: wide metal features dish more than narrow ones.

Why does dimple grinding come before ion milling?

Ion milling removes material slowly. Grinding a dimple first removes most of the material quickly and leaves a thin centre, so the ion milling step is much shorter and causes less beam damage to the sample.

Related pages


Sources


  1. SEMI International Standards: Compilation of Terms (PDF)

More on this topic