Semiconductor Test and Reliability Terms Explained
How chips are tested before and after packaging and how their lifetime is verified: wafer probing, ATE, burn-in, failure analysis and the reliability tests and models behind them.
Proving a chip works
Testing happens twice. Wafer test (probing) screens each die before packaging, using a prober and a probe card connected to automated test equipment. Final test checks packaged parts, often at several temperatures, and system-level test runs real workloads on complex processors.
Reliability testing asks a different question: will the part still work after years in the field? Burn-in, temperature cycling, HAST and electromigration tests accelerate known failure mechanisms so that lifetime can be estimated.
Japanese suppliers
Advantest is one of the two largest ATE makers. Tokyo Electron and Tokyo Seimitsu make wafer probers, and Japanese companies supply probe cards, test sockets and burn-in systems.
All test and reliability terms (43)
- Acceleration Model / Arrhenius EquationFormulas that convert short tests at high temperature, voltage or humidity into equivalent lifetime under normal operating conditions.
- Arrhenius PlotA graph of the log of a reaction or degradation rate against 1/T, whose slope gives the activation energy.
- ATPG (Automatic Test Pattern Generation)EDA software that takes a netlist and fault models and automatically creates test patterns able to detect manufacturing defects.
- Automated Test Equipment (ATE)Computer-controlled testers that apply signals and power to chips, measure the responses and sort good parts from bad at wafer and package level.
- Bathtub Curve / FIT RateThe bathtub-shaped plot of failure rate over time, with early, random and wear-out periods; FIT is the unit for the random failure rate.
- BinningSorting tested chips into categories (bins) by pass or fail, failure type, or performance such as maximum clock speed.
- Built-In Self-Test (BIST)Test circuitry built into a chip that generates its own patterns and checks the results, reducing reliance on external testers.
- Burn-In TestA pre-shipment screen that runs chips hot and at raised voltage so that devices with latent defects fail in the factory instead of in the field.
- Cost of Test (COT)The testing cost per chip, set mainly by equipment cost per hour, test time and how many chips are tested in parallel.
- Design for Testability (DFT)Design techniques that add test circuitry to a chip, such as scan chains and BIST, so manufacturing defects can be found quickly and cheaply.
- DPPM (Defective Parts Per Million)A quality metric counting defective units per million shipped; it measures how many bad chips escape testing and reach customers.
- Electromigration (EM)The gradual movement of metal atoms in interconnects pushed by the flow of electrons, which creates voids and hillocks and eventually breaks or shorts wires.
- ESD Test (HBM / CDM)Tests that measure how much electrostatic discharge a chip can survive, mainly under the human body model and the charged device model.
- Failure Analysis (FA)The work of finding the physical root cause of a failed chip, moving step by step from electrical tests to cross-sections under the microscope.
- Fault CoverageThe share of modelled faults that a set of test patterns can detect; the basic number used to quantify test quality.
- Final TestThe electrical test of chips after packaging that decides whether each unit can ship and which performance grade it belongs to.
- HAST (Highly Accelerated Stress Test)A pressurised high-temperature, high-humidity test that brings out moisture-driven failures in packaged chips in days rather than weeks.
- HTOL (High Temperature Operating Life)An accelerated life test that runs sample devices hot and biased for around 1,000 hours to estimate lifetime and failure rate in FIT.
- IDDQ TestA test that measures a CMOS chip's supply current while it is idle and rejects chips whose current is abnormally high.
- Kelvin Connection (Four-terminal Sensing)A measurement method that uses separate force and sense wires so lead and contact resistance do not distort small resistance readings.
- Latch-upA failure in which a parasitic thyristor inside CMOS turns on and shorts the supply to ground, often destroying the chip.
- MSL (Moisture Sensitivity Level)A JEDEC rating from 1 to 6 that sets how long a surface-mount package can be exposed to room air before it must be soldered or baked.
- OBIRCH (Optical Beam Induced Resistance Change)A failure-analysis method that scans a laser over a biased chip and maps where heating changes the current, revealing shorts and leaks.
- Parametric Test (DC Test)A test that measures a chip's voltages and currents directly and checks that each value falls inside its specified limits.
- Pin ElectronicsThe per-pin circuits in a tester that drive signals, judge outputs, load pins and measure DC currents and voltages.
- Probe CardA product-specific fixture whose fine needles touch the pads of every die on a wafer so the tester can check them electrically before dicing.
- Probe Mark (Scrub Mark)The scratch left on a bond pad when a probe card needle is pressed and slid across it during wafer test.
- RF Test (S-parameters)Testing of chips that handle radio-frequency signals, measuring S-parameters, gain, noise, distortion and modulation quality.
- Silent Data Corruption (SDC)When a CPU or GPU produces wrong results without raising any error, usually because of a subtle defect missed in test.
- Soft ErrorA temporary bit flip in memory or a latch caused by radiation such as alpha particles or cosmic-ray neutrons; the chip is not damaged.
- Strobe (Tester Compare Timing)The point in each test cycle at which automatic test equipment samples a device output and compares it with the expected value.
- System Level Test (SLT)A test that runs a packaged chip with real software and workloads, catching defects that structural ATE tests miss.
- Temperature Cycle Test (TCT)A reliability test that repeatedly swings packaged devices between cold and hot to reveal cracks and delamination from thermal expansion mismatch.
- Test HeadThe part of automatic test equipment placed right next to the device, holding the pin electronics and power supply boards.
- Test Socket / ContactorThe contact part that connects a packaged chip's terminals to the test board during final test; the packaged-device counterpart of a probe card.
- Test Vector / Test PatternCycle-by-cycle lists of input values and expected outputs that a tester applies to a chip to decide whether it passes.
- THB Test (Temperature Humidity Bias)A reliability test that stores biased packages at 85 °C and 85% relative humidity for about 1,000 hours to check moisture resistance.
- Time-Dependent Dielectric Breakdown (TDDB)A wear-out failure in which a gate dielectric under constant electric field suddenly loses its insulation after a period of time.
- Tin WhiskerThin, needle-like crystals that grow from tin plating over time and can short adjacent terminals.
- Wafer Test (Wafer Sort)The electrical test of every die while it is still on the wafer, done with a prober, probe card and tester before dicing and packaging.
- Wafer-Level Burn-In (WLBI)Burn-in done on whole wafers before packaging, applying heat and voltage to weed out chips likely to fail early.
- Weibull DistributionA probability distribution for product lifetimes whose shape parameter shows whether failures are early, random or wear-out.
- Zero Defect (ZD)A quality philosophy that aims for no defects at all, building quality into design, manufacturing and test rather than tolerating failures.
Test and reliability comparisons
Related pages
Glossary
Test and reliability terms
- Acceleration Model / Arrhenius Equation
- Arrhenius Plot
- ATPG (Automatic Test Pattern Generation)
- Automated Test Equipment (ATE)
- Bathtub Curve / FIT Rate
- Binning
- Built-In Self-Test (BIST)
- Burn-In Test
- Cost of Test (COT)
- Design for Testability (DFT)
- DPPM (Defective Parts Per Million)
- Electromigration (EM)
- ESD Test (HBM / CDM)
- Failure Analysis (FA)
- Fault Coverage
- Final Test
- HAST (Highly Accelerated Stress Test)
- HTOL (High Temperature Operating Life)
- IDDQ Test
- Kelvin Connection (Four-terminal Sensing)
- Latch-up
- MSL (Moisture Sensitivity Level)
- OBIRCH (Optical Beam Induced Resistance Change)
- Parametric Test (DC Test)
- Pin Electronics
- Probe Card
- Probe Mark (Scrub Mark)
- RF Test (S-parameters)
- Silent Data Corruption (SDC)
- Soft Error
- Strobe (Tester Compare Timing)
- System Level Test (SLT)
- Temperature Cycle Test (TCT)
- Test Head
- Test Socket / Contactor
- Test Vector / Test Pattern
- THB Test (Temperature Humidity Bias)
- Time-Dependent Dielectric Breakdown (TDDB)
- Tin Whisker
- Wafer Test (Wafer Sort)
- Wafer-Level Burn-In (WLBI)
- Weibull Distribution
- Zero Defect (ZD)
- Wafer test vs final test: what is the difference?
- HTOL vs burn-in: what is the difference?
Last updated: November 1, 2026